Prior art keywords
composition
groups
value
water
emulsion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Abandoned
Application number
CA002003748A
Other languages
French (fr)
Inventor
William John Raleigh
Raymond Joseph Thimineur
Anthony Arthur Zotto
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
General Electric Co
Original Assignee
General Electric Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by General Electric Co filed Critical General Electric Co
Publication of CA2003748A1 publication Critical patent/CA2003748A1/en
Abandoned legal-status Critical Current

Links

Classifications

    • AHUMAN NECESSITIES
    • A61MEDICAL OR VETERINARY SCIENCE; HYGIENE
    • A61KPREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES
    • A61K8/00Cosmetics or similar toiletry preparations
    • A61K8/02Cosmetics or similar toiletry preparations characterised by special physical form
    • A61K8/04Dispersions; Emulsions
    • A61K8/06Emulsions
    • AHUMAN NECESSITIES
    • A61MEDICAL OR VETERINARY SCIENCE; HYGIENE
    • A61KPREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES
    • A61K8/00Cosmetics or similar toiletry preparations
    • A61K8/02Cosmetics or similar toiletry preparations characterised by special physical form
    • A61K8/04Dispersions; Emulsions
    • A61K8/06Emulsions
    • A61K8/064Water-in-oil emulsions, e.g. Water-in-silicone emulsions
    • AHUMAN NECESSITIES
    • A61MEDICAL OR VETERINARY SCIENCE; HYGIENE
    • A61KPREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES
    • A61K8/00Cosmetics or similar toiletry preparations
    • A61K8/18Cosmetics or similar toiletry preparations characterised by the composition
    • A61K8/72Cosmetics or similar toiletry preparations characterised by the composition containing organic macromolecular compounds
    • A61K8/84Cosmetics or similar toiletry preparations characterised by the composition containing organic macromolecular compounds obtained by reactions otherwise than those involving only carbon-carbon unsaturated bonds
    • A61K8/89Polysiloxanes
    • A61K8/891Polysiloxanes saturated, e.g. dimethicone, phenyl trimethicone, C24-C28 methicone or stearyl dimethicone
    • A61K8/894Polysiloxanes saturated, e.g. dimethicone, phenyl trimethicone, C24-C28 methicone or stearyl dimethicone modified by a polyoxyalkylene group, e.g. cetyl dimethicone copolyol
    • AHUMAN NECESSITIES
    • A61MEDICAL OR VETERINARY SCIENCE; HYGIENE
    • A61QSPECIFIC USE OF COSMETICS OR SIMILAR TOILETRY PREPARATIONS
    • A61Q15/00Anti-perspirants or body deodorants
    • AHUMAN NECESSITIES
    • A61MEDICAL OR VETERINARY SCIENCE; HYGIENE
    • A61QSPECIFIC USE OF COSMETICS OR SIMILAR TOILETRY PREPARATIONS
    • A61Q19/00Preparations for care of the skin
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08GMACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
    • C08G77/00Macromolecular compounds obtained by reactions forming a linkage containing silicon with or without sulfur, nitrogen, oxygen or carbon in the main chain of the macromolecule
    • C08G77/04Polysiloxanes
    • C08G77/38Polysiloxanes modified by chemical after-treatment
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08GMACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
    • C08G77/00Macromolecular compounds obtained by reactions forming a linkage containing silicon with or without sulfur, nitrogen, oxygen or carbon in the main chain of the macromolecule
    • C08G77/42Block-or graft-polymers containing polysiloxane sequences
    • C08G77/46Block-or graft-polymers containing polysiloxane sequences containing polyether sequences
    • CCHEMISTRY; METALLURGY
    • C09DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
    • C09KMATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
    • C09K23/00Use of substances as emulsifying, wetting, dispersing, or foam-producing agents
    • CCHEMISTRY; METALLURGY
    • C09DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
    • C09KMATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
    • C09K23/00Use of substances as emulsifying, wetting, dispersing, or foam-producing agents
    • C09K23/54Silicon compounds
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10STECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10S424/00Drug, bio-affecting and body treating compositions
    • Y10S424/05Stick

Abstract

IMPROVED SILICONE SURFACTANTS

Abstract of the Disclosure Novel polysiloxane polymers are provided having general formula wherein R1 is a polyoxyalkylene radical of the formula

Description

200374~

INPROVED SIEICONE SURFACTANTS

The present invention relates to novel polysiloxane-polyether copolymers and their use in stabilizing water-in-oil emulsions, such as polishes and antiperspirant compositions of the so-called dry-feeling type, comprising an emulsion of water in avolatile, water-insoluble liquid.

BACRGROUND OF THE IN~ENTION
A variety of polysiloxane-polyether or polysiloxane~polyoxyalkylene copolymers is known to the art, and the copolymers have found many uses including the manufacture of polyurethane foams and emulsification of one of a pair of immiscible liquids in the other, such as water-in-oil, oil-in-water and oil-in-oil emulsions.
The use of polysiloxane surface active agents comprising organic polyether groups to stabilize emulsions is well known. U.S. Patent No. 4,265,878, issued May 5, 1981 to Keil, uses a polysiloxane surface active agent to stabilize antiperspirant stick 20 compositions. U.S. Patent No. 4,218,250, issued ~ugust 19, 1980 to Kasprzak, uses such a polysiloxane surface active agent to stabilize polish formulations. U.S.
Patent No. 4,268,499, issued May 19, 1981 to Keil, uses such surface active agents to stabilize antiper~pirant emulsion compositions. Further, U.S. Patent No.
4,311,695, issued January 19, 1982 to Starch, uses such surface active agents in personal care creams and the like.
Polysiloxane surface active agents are sometimes referred to as polysiloxane-polyoxyalkylene copolymers. However, their use to date as stabilizers for silicone emulsions, particularly water-in-oil emulsions, has not always been completely satisfactory because the variables affecting their function are not well understood. Water-in-oil emulsions which contain high concentrations of salts or other ionic materials are often particularly difficult to stabilize. The problems encountered in formulating emulsions of anti-perspirants in volatile fluids are exemplary of this.
Antiperspirant compositions are well known in the cosmetic art. These compositions are formulated as aerosols, gels, sticks, creams, pump sprays and lotions and comprise an astringent, typically comprising one or more zirconium salts and/or aluminum salts, in various forms such as a dry, impalpable powder, in alcohol solution or an aqueous solution. Of these various forms of astringents the aqueous solution is generally considered to be the most effective antiperspirant.
An antiperspirant composition having water as the continuous phasej such as an aqueous solution of an astringent, or an oil-in-water type emulsion thereof, is less desirable because it tends to feel wet when applied to the human skin and to go through a tacky state during the drying period after application. Therefore the use of water-in-oil emulsions to apply antiperspirants to the skin has found favor.
U.S. Patent No. 4,122,029, issued October 24, : : .
~ 35 1978 to Gee et al, discloses water-in-oil type ~

2003~48 compositions having broad utility and comprising a polydiorganosiloxane-polyoxyalkylene copolymer and a water-in-oil type surfactant. When formulated as an antiperspirant emulsion of an aqueous solution of an `~
astringent such as aluminum chlorhydrate emulsified in a volatile, non-aqueous continuous phase, these compositions have a desirable dry feeling when applied to the human skin.
The aforementioned U.S. Patent No. 4,268,499 discloses compositions described as having greater efficacy than those of the aforementioned U.S. Patent 4,122,029. The efficacy was determined by applying compositions to subjects' wrists and measuring the time required for the compositions to begin to dry and turn white.
Another type of water-in-oil emulsion which has found favor with the public is polishes, particularly for furniture. One drawback to furniture polishes which utilize organic or organosilicon surfactants comprising long chain oxyalkylene residues, particularly long chain oxyethylene residues, is that the surfactant may tend to attack the finish of the article to be polished. This is particularly the case when the finish is based on nitrocellulose lacquers since glycol ethers are solvents of choice for nitrocelluIose finishes.

SUMNARY OF THE INVENTION :
It is an object of the present invention to produce novel polysiloxanes containing organic polyether groups.
It is another object of the invention to provide stable emulsions of polar liquids in non-polar liquids.
It is another object of this invention to ,.,. , . ,, : . . . .

: . - -............ . . . .~ -.

provide stable emulsions of polar liquids in low-viscosity polydimethylsiloxanes.
It is another object of this invention to provide stable emulsions of aqueous solutions in low-viscosity polydimethylsiloxanes.
It is another object of the present invention to produce polysiloxane surface active agents for use in formulating polishes, sun screen oils, antiperspirant sticks and lotions, body lotions and the like.
These and other objects are realized by the compositions of this invention wherein a polar liquid is dispersed in a non-polar base liquid by the action of a mixture comprising certain novel polydiorganosiloxane-polyoxyalkylene copolymers.
The polar liquid, which is insoluble in the non-polar base liquid, is the dispersed phase and the base liquid is the continuous phase in the compositions of the invention.
Compositions of this invention wherein the polar liquid comprises water, such as aqueous solutions of personal care products such as insect repellents and antiperspirants and the base liquid comprises a poly-dimethylsiloxane, such as cyclopolydimethylsiloxanes, are of particular interest because of the aesthetic value of the feel of said composition when applied to the human skin DETAILED DESCRIPTION OF T~E INVENTION
The novel polysiloxane polymers of the invention comprise polymers of the general formula (I):
R _ - R R
R2 _ Si ~ t Ri ~ Si ~ ~ si - R2 (I) : ....
,'""~' ' wherein each R individually is an alkyl radical having from 1 to 4 carbon atoms;
R1 is a polyoxyalkylene radical of the formula (II):

- C = C - C - ~ R3 0~ R4 ( I I ) CH3 n wherein each R3 individually is an alkylene radical having from 2 to 6 carbon atoms, R4 iS chosen from the group consisting of R, acyl groups having from 2 to 12 carbon atoms, and hydrogen, and n has an average value of from at least 1 to about 200;
each R2 individually is chosen from the group consisting of R and Rl;
x has an average value of from about 5 to about 400: and y has an average value of at least 1 except that when R2 is Rl, y may be zero.
The groups represented by R in formula ~
include alkyl radicals such as methyl, ethyl, butyl and the like. It is~preferred that at least 80 mole percent of the R groups be methyl.
In the polyoxyalkylene radicals R1 represented by formula (II), the oxyalkylene groups represented by R30 suitably include -CH2CH20-(oxyethylene), -CH2CH(CH3)0- (oxypropylene), CH2C(CH3~2Q-, -(CH2)50- and the like. For many applications it is preferred that at least 50% by number of R30 radicals be oxyethylene. In applications where the surface active agents of the invention are to be utilized to prepare water-in-oil emulsions it is preferred~that all of the R30 radicals :: :

20037~8 be oxyethylene. The balance between oxyethylene and higher oxyalkylene groups such as oxypropylene in the polyether radical (II) may be utilized to alter the degree of hydrophilicity of the surfactant of the invention. When the polyether is all oxyethylene groups, maximum hydrophilicity is achieved. As more of the hydrophobi~ higher oxyalkylene groups are introduced, the hydrophilic nature of the polyether decreases and thus that of the polysiloxane polyoxy-alkylene copolymer surfactant.
In formula (II), R4 is the terminal group ofthe polyoxyalkylene radical Rl. The nature of R4 is not critical and R4 may be chosen from R groups such as methyl, ethyl and the like, acyl groups such as acetyl, and hydrogen. However, when the polysiloxane-polyoxyalkylene copolymer is used to stabilize water~
in-oil emulsions, it is preferred that R4 be hydrogen.
The average value of n, the length of the oxyalkylene chains in formula tII), is not critical and may vary broadly from at least 1 to 200 or more.
The value of n selected for a particular application will be determined largely by the surfactant properties desired in the product as discuss2d below.
It should be recognized that as the length of the oxyalkylene chains increases, the viscosity of the polyether-polysiloxane will increase, and it may be convenient or even necessary to dilute the surfactant with relatively inert solvents when n is very large.
The average value of x in formula (I) also is not critical and may be varied from about 5 to 400 or more. It should be recognized that as x increase the viscosity of the polyether-polysiloxane will increase, an~d at higher values of x it may be convenient or even necessary to dilute the surfactant with relatively inert solvents such as hydrocarbon ,: . .

-. .,-. ,,, . :
: - . . ~ . . ~:

solvents, cyclic polysiloxanes such as octamethyl-cyclotetrasiloxane, polyoxyalkylene ethers and the like as are well-known to the art.
The average value of y in formula (I) likewise is not critical but must be at least 1 except that when R2 is Rl, y may be zero. The utility of unsubstituted polysiloxane polymers as "anti-surfactants in breaking emulsions is well known.
When R2 is R, as the average value of y is reduced toward 1, it is statistically possible that in some polymer molecules y will be zero. These homopolymer molecules may interfere with the surfactant activity of the bulk polymer and reduce the effectiveness of the surfactants for some applications. Therefore, when R2 is R it may be advisable to design or formulate the surfactants for such uses in a manner that will lead to an average value of y somewhat qreater than 1.
The surfactant properties of individual ~-polyether-polysiloxanes of the invention of general formula (I) are governed by the balance chosen between the number of hydrophobic diorganosiloxy groups (the value of x), the number of relatively hydrophilic polyoxyalkylene chains Rl (the value of y), the nature of the oxyalkylene groups R30 in the radical represented by Rl, and the average number of oxyalkylene groups n in each chain. For example, a polyether-polysiloxane~of the invention may be made more hydrophilic by increasing the value of y with respect to x, thereby ~increasing the concentration of hydrophilic polyoxyalkylene groups with respect to diorganosiloxy groups, by increasing the concentration of relatively hydrophilic oxyethylene groups with respect to higher oxyalkylene groups in R1, or ;~
; 35 increasing the number of oxyalkylene groups in the 2[)03~8 chain (the value of n), or combinations thereof. To decrease the hydrophilicity o~ a surfactant, the reverse of the above principles would be applied.
Those skilled in the art of polyether-polysiloxane surfactants are able to develop polymers suitable for particular applications by utilizing the above criteria without undue experimentation.
The polyether-polysiloxane copolymers (I) of the invention are prepared by reaction of polyoxyalkylene ethers of the general formula (III):

HC 9 C - C - 0 (R3 ~ R4 (III) where n, R3 and R4 are as in general formula (II) above, with hydrogen-containing polysiloxanes corresponding to the general formula (I) but where all Rl groups are hydrogen, using a platinum catalyst such as chloroplatinic acid as is well known in the art.
The disclosures of U.S. Patent Numbers 3,657,305, issued April 18, 1972 to Morehouse; 3,234,252, issued February 8, 1966 to Pater; 4,047,958, issued 20 September 13, 1977 to Yoneyama et al; 3,427,271, issued February 11, 1969 to McKellar and 2,846,458, issued August 5, 1958 to Haluska further describe methods for reacting unsaturated polyethers with hydrogen-containing polysiloxanes to prepare polyether-polysiloxane copolymers.
It must be understood that the silicon-bonded hydrogen groups are intended to be completely reacted in the preparation of the copolymers of the invention, but trace amounts may escape reaction and be identifiable in the polyether-polysiloxane polymers of the invention. The preferred method is to use the ~' - , . .: i: : ., . . ;

2003~48 unsaturated polyether in more than stoichiometric amounts to ensure complete reaction of the silicon-bonded hydrogen. This in turn means that the product of the invention may contain some unreacted polyoxy-alkylene ether.
The polyoxyalkylene ethers of general formula (III) above may be prepared by initiating the polymerization of one or more alkylene oxides using the acetylenic alcohol 3-methylbut-1-yn-3-ol (IV) as a starter fH3 HC - C - C - OH (IV) using acidic or basic catalysts as is well known to the art. On completion of the polymerization reaction, the polyether product will correspond to the general formula (III) where R4 is hydrogen. In general, if other end groups R4 are desired, they are introduced by the known methods for etherification ~;
(when R4 is alkyl) or esterification (when R4 is acyl).
The water-in-oil emulsions of the invention comprise:
(a) a polar~liquid, optionally containing dissolved inorganic salt(s) as a discontinuous phase;
(b) a volatile llquid having a normal boiling point less than 250C as a continuous phase, said volatile liquid~ being selected from the group consisting of methylsiloxane fluids having the average unit formula (CH3 ) asio ( 4-a) /2 wherein a has an average value of from 2 to 3 inclusive and paraffinic hydrocarbon fluids; ~

:
~;

:, : , .:

- ~

;~00~74~3 - lO - 60SI-1195 (c) a polydiorganosiloxane-polyoxyalkylene copolymer of the general formula (I) described above;
and optionally, (d) an organic oil-in-water type surfactant having an HLB value of from 8 to 18 inclusive.
Polar liquid (a) of the compositions of this invention is the dispersed phase therein and may comprise one or more efficacious components such as an antiperspirant, a humectant, an insect repellent, an odorant, a deodorant, an emollient, an antiseptic, a sunscreen agent, a cleansing agent, a suitable pharmaceutical, or the like.
The polar liquid (a) may be any suitable liquid composition which is insoluble at room temperature in the base oil, hereinafter described.
By polar it is meant a substance which has a permanent dipole moment. Of course, to maintain the identity of the compositions of this invention the polar liquid should not undergo chemical reaction with remaining components of the composition. The polar liquid may be a pure liquid or a liquid solution or a mixture of immiscible liquids, the components of which are polar and insoluble in the base oil. Solid polar materials may be used as component (a) if they are changed to a - -25 liquid form such as by heating to melt the solid or by ;
dissolving the solid in a solvent. -~
Examples of suitable materials which are polar include inorganic materials such as water, salts, weak acids, weak bases, and aqueous solutions thereof, and organic materials bearing polar groups such as organic compounds bearing nitrogen containing groups such as in amides, amines, amine salts, nitriles, imides, imines, lactams, and nitro compounds; oxygen-containing groups such as in ethers, alcohols, and in carbonyl groups such as in ketones, ''~ ' ' ~ ' : . , :: : . :

- :

aldehydes, carboxylic acids and their salts, esters and lactones; phosphorus-containing groups such as in phosphates and phosphonium salts; sulfur-containing groups such as in sulfones, mercaptans, sulfoxides and sulfides; and halogens such as in hydrocarbon chlorides, bromides, and iodides. The presence of said polar groups in the organic material provides a permanent dipole moment and thus provides the polar character in the organic material.
lo Emulsion compositions of this invention wherein the polar liquid comprises water and/or ethanol are particularly useful. In common with oil-in-water emulsions, water-in-oil emulsions are desirable from an economic safety and environmental viewpoint as a means of preparing, storing, shipping, and using efficacious components. In addition, emulsion compositions of aqueous or ethanolic solutions in methylsiloxane fluids have value as personal care compositions, as noted above.
Polar liquids (a) of particular interest for the compositions of this invention are therefore selected from the group consisting of water, water solutions of polar solutes, polar liquids soluble in water, ethanol, ethanol solutions of polar solutes and polar liquids soluble in ethanol. Suitable water solutions comprise, as the polar solute, inorganic solutes hereinbefore exemplified and organic solutes such as alcohols such as methanol, ethanol, phenol, ethylene qlycol, propylene glycol, glycerine, and their partial ethers and partial esters; nitrogen compounds such as amides such as formamide, acetamide, N-methylacetamide, N,N-dimethyl formamide and urea, nitriles such as acetonitrile and amines and their salts, acids such as formic acid, acetic acid, benzoic acid, stearic acid, and ethylenediaminetetracetic ' .
:. .
. .
~ : : : :: - . : .

: . ; :: ~ :

Z~03748 - 12 - 60SI-~195 acid and ethers such as furan, tetrahydrofuran, dioxane, ethylene glycol dimethyl ether, propylene glycol dimethyl ether and their polymeric forms such as triethylene glycol diethyl ether. Suitable ethanol solutions comprise any suitable ethanol-soluble inorganic or organic solute exemplified above as the solute as well as other polar solutes which are insoluble in water but soluble in ethanol such as 2-ethyl-1,3-hexanediol, N,N-diethyltoluamide and lo 2-ethylhexyl-p-dimethylaminobenzoate.
The base oil or volatile liquid (b) is a fluid selected from the methylsiloxane fluids having a normal, i.e. atmospheric pressure, boiling point of less than 250C, a paraffinic hydrocarbon, or their mixtures. The volatile methylsiloxane fluid (b) has the average unit formula (CH3)aSiO(4-a)/2 where a has an average value of from 2 to 3 and consists of siloxane units selected from the group consisting of (CH3)3Siol/2 (cH3~sio2/2~ CH3sio3/2 and sio4~2 units. Preferably, the volatile methylsiloxane fluid consists essentially of dimethylsiloxane units, and optionally, trimethylsiloxane units. Of particular value as volatile liquid (b) are the cyclic siloxanes of the general formula [(CH3)2Sio]b and the linear siloxanes of the general formula (CH3)3S io [ CH3)2si]csi(CH3)3, and their mixtures, wherein b is an integer of from 3 to 6 and c is an ;
integer of from 0 to 4. A highly preferred methylsiloxane fluid is a mixture of said cyclic siloxanes wherein a major portion is tetramer (b=4). ~ ;
Paraffinic hydrocarbon fluids suitable for use in these compositions correspond to the average unit formula CnH2n+2, wherein n is an integer having a value such that the paraffinic hydrocarbon is fluid at : ~ :

;~03748 room temperature. of particular value as a base liquid in volatile compositions are the paraffins having a value of n less than 15 such as kerosene, gasoline, and the gaseous paraffins. Of course, gaseous paraffins, in order to be operative in the dispersions of this invention, must be used at low temperature and/or super-atmospheric pressure to keep them in the liquid state.
The base oil, in addition to being a methyl-siloxane fluid or a paraffin, may be any mixture ofsaid methylsiloxane fluid and said paraffin such as a mixture of octamethylcyclotetrasiloxane and hexane or decamethylcyclopentasiloxane and butane or a mixture of two or more of said cyclosiloxanes and one or more paraffins.
Component (c) is a polydiorganosiloxane-polyoxyalkylene copolymer preferably containing polydimethylsiloxy groups, and on average at least one polyoxyalkylene group, having the general formula ~I) described above.
Component ~d) is any cationic, anionic or nonionic organic surfactant suitable for preparing emulsions of the oil-in-water type and having an HLB
value of from 8 to 18, inclusive. Examples of ~5 oil-in-water type surfactants include polyethoxylated quaternary ammonium salts and polyoxyethylene fatty amines as cationic surfactants, and polyethylene-glycol alkylethers, polyethyleneglycol alkylaryl-ethers, polyethyleneglycol alkylarylethers, polyethoxylated sorbitan monolaurate, polyethoxylated sorbitan monooleate, polyoxyethylene lanolin derivatives, and polyethoxylated fatty alcohols as nonionic surfactants. Mixtures of cationic and/or nonionic oil-in-water surfactants are also suitable.
Other examples of suitable organic surfactants having .: . . . '' , ' - :': . - ' ' - . - .- ~ ~ ...... . . . ~ , . .
- . . . - . ~ ~ ~

an HLB value of from 8 to 18 may be found by consulting standard publications such as McCutcheon's ~Detergents and Emulsifiers" 1975 North America Edition, MC Publishing Co., Glen Rock, NJ 1975.
The amounts of components (a) and (b) that may be present in the compositions of this invention may vary widely and comprise, in total, from 99.5 to 91 percent by weight of the total weight oE components (a) through (d). The polar liquid (a) may comprise from 89.5 to 50~ preferably 85 to 60, weight percent of components (a) through (d); the volatile liquid (b) comprises fro~ 10 to 45, preferably 15 to 35 weight percent of the total weight of components (a) to (d).
The surfactant mixture, consisting essentially of component (c) and optionally (d) comprises, in total, from 0.5 to 9 percent by weight of the total weight of components (a) and (d), with component (c) accounting for from 0.5 to 6 weight percent of the total of components (a) to (d).
The compositions of this invention may further comprise additional components useful in consumer products which are insoluble in the polar :~
phas~. Examples o~ such components include waxes;
colorants; perfumes; viscosity control additives, such as solvents or thickening agents for the continuous phase; and non-volatile organopolysiloxanes, such as polydimethylsiloxanes having a viscosity of from 5 to 10,000 centipoise at 25C.
The compositions of this invention may be prepared by mixing the proper portions of the individual components in any order. Although the compositions of the invention delineated in terms of a : polar liquid (a) emulsified in a volatile liquid, (b), using a mixture of surfactants, (c) and (d), the .
following examples employ the preferred method of :

. ~, :, . . ., , .,. . , .. .. - ... .. . .

preparing a so-called polar or aqueous phase (a) and any oil-in-water type surfactant (d) and preparing a so-called oil phase comprising the volatile liquid (b) and the polydiorganosiloxane-polyoxyalkylene copolymer (c) and thereafter mixing the so-called aqueous phase with the so-called oily phase. If any component is a solid, it is converted to a liquid form by melting or dissolving before the emulsion is formed. Mixing may be done using standard emulsifying methods.
In order that those skilled in the art may better understand how the present invention can be practiced, the following specific components and examples are disclosed for purposes of illustrating and not limiting the invention. All percentage and parts are by weight, and all viscosities were measured in centipoise at 25C.
EXPERINENTA~
Examples 1-8 The copolymers of Examples 1-8 were prepared from trimethylsiloxy end blocked polysiloxanes containing methylhydrogensiloxy units of the general formula (CH3)3sio-[(CH3)2si-]x[(CH3)HSio-]ySi(CH3)3 having values of "x" and "y" as shown in Table I.
These polysiloxanes are readily prepared by equilibration of appropriate (stoichiometric) amounts of hexamethyldisiloxane, a cyclic telomer of dimethyl-siloxy qroups and a telomer of methylhydrogensiloxy groups as is well known in the art~
The polysiloxane-polyether copolymers were prepared in the following manner. A known amount of starting polysiloxane containing methylhydrogensiloxy groups was charged to a reactor with an equal amount .

. : - . . - : . - , : .

- 16 - 60SI-llg5 of toluene. The mixture was refluxed to remove toluene-water azeotrope, decanting and recycling the toluene to the reactor until the mixture was dry. The system was cooled to 100C and a small amount (about 1% on reactants) of a 0.2N solution of sodium acetate in methanol/isopropanol was added, followed by approximately 0.04~ on reactants of a solution of chloroplatinic acid in octanol containing 3.5%platinum. Over a period of about an hour 2-(3-methyl-3-butynoxy)ethanol, "MBEO 1.8 Adduct", manufactured by Air Products and Chemicals, Inc., Allentown, PA, corresponding to the polyether group desired in the product in a quantity equal to 110% of the stoichiometric amount was fed to the reactor with stirring. The mixture was held at 100C with stirring for an additional 4 hours. The toluene was then stripped under vacuum with heating until the temperature of the mixture reached 130C at 10mm Hg pressure. The product was then cooled, filtered, and stored until used.
TABLE I
"x" "y"% Silicone~ Polyether Example 1 15 1 78 22 25 Example 2 10018 73 27 ~-Example 3 20035 73 27 Example 4 10030 64 36 Example 5 100 3 94 6 Example 6 10 1 84 16 30 Example 7 20 6 65 35 Example 8* 0 20 27 73 ;~

* Product gelled, probably because side reactions between terminal hydroxyl and silanic hydrogen caused significant cross-linking.

;~

:, . . .
, 20037~a - 17 - 60SI-lls5 The surfactants of E'xamples 1-3 were each formulated into the antiperspirant emulsions shown in Table II.

TABLE II
Ingredient Formulation A B
Octamethylcyclotetrasiloxane 15.0 20.0 Surfactant (10% in octamethyl- 16.5 11.0 cyclotetrasiloxane) Polysorbate 80 0.2 0.13 Aluminum zirconium chlorohydrate glycine complex (Wickenol 369)TM 20.0 20.0 Water 48.3 48.~37 15 In each instance the surfactant was combined with octamethylcyclotetrasiloxane to form an oil phase. Wickenol 369TM, Polysorbate 80TM and water were combined in the aqueous phase. The aqueous phase was added to the oil phase with good mixing until a homogeneous emulsion formed. Then this mixture was homogenized on a Polytron at 13,000 RPM for 30 seconds. The batch size in each case was between 400-500 grams.
The emulsions were examined for stability at room temperature and at 50C. The emulsions prepared with the surfactant of Example 1 had marginal stability, perhaps because when the average value of "y" is one, the surfactant contains a significant concentration of polydimethylsiloxane, which may destabilize the emulsion. The emulsions prepared with the surfactants of Examples 2 and 3 were stable at both temperatures.

:
.
-: ~ , - ,. : -:

;~:100374~3 EX~P~E 10 A water-in-oil emu]sion useful as a furniture polish was prepared in the following fashion using the product of Example 7 as the emulsifier.

Material Parts by Weight Part A
Water 59.6 Wax emulsion containing 3.5 Oxidized microcrystalline wax 20.0 Oleic acid 3.0 Morpholine 4.0 Water 73.0 100. 0 Material Parts by Weight Part B
Mineral spirits (1) 32.5 Polydimethylsiloxane oil (500 cps) 1.7 Polydimethylsiloxane oil (1000 cps) 1.7 Product of Example 7 1.0 100.0 ~1) Use of a deodorized hydrocarbon such as Isopar C
or E would be preferred.
~ , First the components of Part A and Part B were each blended separately, and then Part A was added to Part B with high speed agitation.
In typical fashion the resulting polish separated slightly on prolonged standing but redispersed easily with gentle shaking. When applied to a surface, t:he emulsion broke quickly on rubbing the surface ~with a soft cloth and imparted an esthetically pleasing polished appearance to the ~ -surface. Perhaps because the polyether side chain . :
~ ' ~; - . . ~ . . . .
: . ~ : . : . ,.............. . :

20037~a8 is hydroxyl-terminated and/or because the ether side chain is short, the polish shows a reduced tendency to attack a nitrocellulose-based finish.

A stick antiperspirant composition was prepared using the product of Example 4 as the emulsifier.

MaterialParts by Weight Part A
10 Octamethylcyclotetrasiloxane24.00 Product of Example 7 1.00 Stearyl alcohol 11.25 Methyl Hydroxy Stearate (Paricin 1) 3.75 Talc 7.50 15Polysorbate 81 (Tween 81) 0.10 Part B
Aluminum-zirconium tetrachlorohydrate glycine salt (Wickenol 369) 25.00 Water 27.40 100.00 ~ ;

The components of Part A were mixed together and warmed to 60C until all the wax melted, using mild stirring to ensure a homogeneous mixture. The components of Part B were also warmed to 60C and added tc Part A with~moderate agitation. When the emulsion became homogeneous, it was cooled to 52C
while continuing mixing. The preparation was then poured into suitable containers and allowed to cool to ambient temperature. The resulting antiperspirant stick was uniform in appearance and had good consistency, but additional formulation work should be :'~
: : . . . - : ` ~ ` ; !

. .

2~03748 required to optimize the strength of the stick.

A water-in-oil emulsion cosmetic composition such as is used for a body or night cream was prepared using the product of Example 4 as the emulsifier.

Material Parts by Weight Part A
Mineral oil 15.0 Mixture of Mineral Oil, Petrolatum, Ozokerite, Glyceryl Oleate and Lanolin Alcohol (Protegin X) 5.0 Product of Example 2.0 ' Part B
Polysorbate 80 0.4 15 Sodium Chloride 2.0 Water 75.6 ~-100. 00 ;

The elements of Parts A and B were separately mixed.~ Then Part B was added to Part A
with high speed mixing. The resulting;emulsion had a ` 20 smooth creamy composit~ion which was ea~sily spread on the skin. Care to avoid overmixing must be taken, as overmixing tends to cause the emulsion~to invert to an oil-in-water system.

.

-~ :

Claims (13)

1. A polysiloxane surface active agent comprising polymers of the general formula (I):

(I) wherein each R individually is chosen from the group consisting of alkyl radicals having from 1 to 4 carbon atoms; R1 is a polyoxyalkylene radical of the formula (II) wherein each R3 individually is an alkylene radical having from 2 to 6 carbon atoms, R4 is chosen from the group consisting of R, acyl groups having at last 2 carbon atoms, and hydrogen, and n has a value from at least 1 to about 200, each R2 individually is chosen from the group consisting of R and R1; x has a value from about 5 to about 400; and y has a value of at least 1 except that when R2 is R1, y may be zero.
2. The composition of claim 1 wherein at least 80 mole percent of the R groups is methyl.
3. The composition of claim 1 wherein at least 50 percent by number of the R3O groups is oxyethylene.
4. The composition of claim 1 wherein 100 percent of the R3O groups is oxyethylene.
5. The composition of claim 1 wherein n is about 1.8.
6. The composition of claim 1 wherein at least 80 mole percent of the R groups is methyl, 100 percent of the R3O groups is oxyethylene, and n is about 1.8.
7. An emulsion which comprises the composition of claim 1.
8. A water-in-oil emulsion which comprises the composition of claim 1.
9. An emulsion comprising:
(a) a polar liquid, optionally containing dissolved inorganic salt(s) as a discontinuous phase;
(b) a volatile liquid having a normal boiling point less than 250°C as a continuous phase, said volatile liquid being selected from the group consisting of methylsiloxane fluids having the average unit formula (CH3)aSiO(4-a)/2 wherein a has an average value of from 2 to 3 inclusive and paraffinic hydrocarbon fluids;
(c) the composition of claim 1, and optionally;
(d) an organic oil-in-water type surfactant having an HLB value of from 8 to 18 inclusive.
10. An emulsion comprising:
(a) from 89.5 to 50 parts of a polar liquid, optionally containing dissolved inorganic salt(s) as a discontinuous phase;
(b) from 10 to 45 parts of a volatile liquid having a normal boiling point less than 250°C as a continuous phase, said volatile liquid being selected from the group consisting of methylsiloxane fluids having the average unit formula (CH3)aSiO(4-a)/2 wherein a has an average value of from 2 to 3 inclusive and paraffinic hydrocarbon fluids;
(c) 0.5 to 6 parts of the composition of claim 1; and optionally;
(d) from 0.1 to 3 parts of an organic oil-in-water type surfactant having an HLB value of from 8 to 18 inclusive;
where the total of a + b + c + d is 100 parts.
11. The composition of claim 9 or claim 10 which further comprises a wax.
12. The composition of claim 9 wherein the polar liquid comprises an aqueous solution of an antiperspirant salt.
13. The invention as defined in any of the preceding claims including any further features of novelty disclosed.
CA002003748A 1988-12-29 1989-11-23 Silicone surfactants Abandoned CA2003748A1 (en)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US07/291,909 US5008103A (en) 1988-12-29 1988-12-29 Silicone surfactants
US291,909 1989-12-29

Publications (1)

Publication Number Publication Date
CA2003748A1 true CA2003748A1 (en) 1991-05-23

Family

ID=23122386

Family Applications (1)

Application Number Title Priority Date Filing Date
CA002003748A Abandoned CA2003748A1 (en) 1988-12-29 1989-11-23 Silicone surfactants

Country Status (9)

Country Link
US (1) US5008103A (en)
EP (1) EP0379677B1 (en)
JP (1) JPH02229539A (en)
KR (1) KR0154895B1 (en)
AT (1) ATE125171T1 (en)
AU (1) AU631164B2 (en)
CA (1) CA2003748A1 (en)
DE (1) DE68923545T2 (en)
ES (1) ES2075030T3 (en)

Families Citing this family (39)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4936917A (en) * 1988-01-12 1990-06-26 Air Products And Chemicals, Inc. Water based mold release compositions containing poly(siloxane-glycol) surfactants for making polyurethane foam article in a mold
US5066756A (en) * 1988-12-29 1991-11-19 General Electric Company Silicone surfactants
US4983233A (en) * 1989-01-03 1991-01-08 General Electric Company Fatigue crack resistant nickel base superalloys and product formed
US5162378A (en) * 1990-04-20 1992-11-10 Revlon Consumer Products Corporation Silicone containing water-in-oil microemulsions having increased salt content
JP2986911B2 (en) * 1990-06-25 1999-12-06 エス.シー.ジョンソン アンド サン,インコーポレーテッド Furniture polish concentrates and formulations
JP3033995B2 (en) * 1990-08-03 2000-04-17 オキツモ株式会社 Deodorizer and products using it
DE4032006A1 (en) * 1990-10-09 1992-04-16 Wacker Chemie Gmbh METHOD FOR DEFOAMING AND / OR DEGASSING ORGANIC SYSTEMS
US5387417A (en) * 1991-08-22 1995-02-07 Dow Corning Corporation Non-greasy petrolatum emulsion
US5292503A (en) * 1991-10-09 1994-03-08 General Electric Company Stable water in oil emulsions
CA2077828A1 (en) * 1991-10-10 1993-04-11 William J. Raleigh Silicone polyether alkyl copolymer synthesis
EP0585044B1 (en) * 1992-08-21 1998-12-09 General Electric Company Silicone polyether surfactants
JPH0637385U (en) * 1992-10-16 1994-05-17 株式会社フジカ Throwing tape storage container
US5456906B1 (en) * 1993-11-17 2000-12-05 Gen Electric Antiperspirant compositions
US5531986A (en) * 1994-07-01 1996-07-02 The Mennen Company Low residue antiperspirant solid stick composition
US5534246A (en) * 1994-08-29 1996-07-09 Helene Curtis, Inc. Topically-effective compositions
FR2739775B1 (en) 1995-10-16 1997-11-21 Oreal DEODORANT COMPOSITION COMPRISING A WATER-SOLUBLE SALT OF ZINC AS AN ODOR-ABSORBING AGENT
US5725845A (en) * 1995-11-03 1998-03-10 Revlon Consumer Products Corporation Transfer resistant cosmetic stick compositions with semi-matte finish
US5672338A (en) * 1996-03-14 1997-09-30 General Electric Company Cosmetic compositions made with hydroxy carbamate functionalized silicones
US5686547A (en) * 1996-03-14 1997-11-11 General Electric Company Carbonate and hydroxy carbamate functionalized silicones
JP2000086772A (en) * 1998-09-14 2000-03-28 Ge Toshiba Silicones Co Ltd Water-in-oil type silicone emulsion composition
US5989531A (en) * 1998-11-13 1999-11-23 Colgate-Palmolive Company Antiperspirant formulation for porous applicator
US6685952B1 (en) 1999-06-25 2004-02-03 Unilever Home & Personal Care Usa, Division Of Conopco, Inc. Personal care compositions and methods-high internal phase water-in-volatile silicone oil systems
US6403067B1 (en) 2000-05-19 2002-06-11 Colgate-Palmolive Company Stable emulsions for cosmetic products
US6468511B1 (en) 2000-05-19 2002-10-22 Colgate-Palmolive Company Emulsions with naphthalate esters
US6652867B1 (en) * 2000-09-25 2003-11-25 Dow Corning Corporation Compositions containing organic oil-in-water emulsions, salts, alcohols and solvents
US6387357B1 (en) 2000-10-20 2002-05-14 Colgate-Palmolive Company High oil clear emulsion with diene elastomer
US6403069B1 (en) 2000-10-20 2002-06-11 Colgate-Palmolive Company High oil clear emulsion with elastomer
US6552212B2 (en) 2001-05-14 2003-04-22 Finetex, Inc. Benzoate esters of hydroxyl terminated polyether polysiloxane copolyols and process for producing same
US20030040571A1 (en) * 2001-07-30 2003-02-27 Feng Qian Jane Clear silicone microemulsions formed spontaneously
DE10154627A1 (en) * 2001-11-07 2003-05-15 Beiersdorf Ag Cosmetic or dermatological impregnated wipes
US20050142085A1 (en) * 2003-12-24 2005-06-30 Kao Corporation Antiperspirant and deodorant stick composition
US20070266749A1 (en) * 2006-05-15 2007-11-22 Jason Rader Pesticidal compositions for treating anthropods and methods for the use thereof
US8790673B2 (en) * 2006-05-15 2014-07-29 Oms Investments, Inc. Methods for treating arthropods
US8734821B2 (en) * 2006-05-15 2014-05-27 Oms Investments, Inc. Silicone surfactant-based agricultural formulations and methods for the use thereof
DE102009012074A1 (en) * 2009-01-16 2010-09-23 Acmos Chemie Kg Release agents and their use for the production of polyurethane moldings
KR102131604B1 (en) * 2012-10-11 2020-07-09 다우 실리콘즈 코포레이션 Aqueous silicone polyether microemulsions
US9822280B2 (en) 2013-06-18 2017-11-21 Dow Global Technologies Llc Crosslinkable coating composition and method of producing the same
US10604626B2 (en) * 2013-07-31 2020-03-31 Dow Global Technologies, Llc Process for preparing polycarbamate and reaction product thereof
US9796815B2 (en) * 2013-07-31 2017-10-24 Dow Global Technologies Llc Process for preparing polycarbamate and reaction product thereof

Family Cites Families (18)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US2846458A (en) * 1956-05-23 1958-08-05 Dow Corning Organosiloxane ethers
US3234252A (en) * 1962-10-02 1966-02-08 Union Carbide Corp Siloxane-polyoxyalkylene copolymers
US3427271A (en) * 1966-11-04 1969-02-11 Dow Corning Novel organosilicon compositions
US3779956A (en) * 1969-12-24 1973-12-18 Union Carbide Corp Process for reducing flammability of polyurethane foams
US3686254A (en) * 1969-12-24 1972-08-22 Union Carbide Corp Siloxane-polyoxyalkylene block copolymers
US3933695A (en) * 1972-12-29 1976-01-20 Union Carbide Corporation Hydroxyalkenylsiloxane rigid poly urethane foam stabilizers
GB1522406A (en) * 1975-04-07 1978-08-23 Fuji Photo Film Co Ltd Light-sensitive silver halide photographic materials
US4014825A (en) * 1975-12-29 1977-03-29 Union Carbide Corporation Tertiary alcohol-bearing organosilicone polymers
US4122029A (en) * 1977-07-27 1978-10-24 Dow Corning Corporation Emulsion compositions comprising a siloxane-oxyalkylene copolymer and an organic surfactant
US4218250A (en) * 1978-09-28 1980-08-19 Dow Corning Corporation Polish formulations
US4265878A (en) * 1979-06-07 1981-05-05 Dow Corning Corporation Antiperspirant stick compositions
US4268499A (en) * 1979-06-07 1981-05-19 Dow Corning Corporation Antiperspirant emulsion compositions
US4311695A (en) * 1979-12-03 1982-01-19 Dow Corning Corporation Personal-care emulsions comprising a siloxane-oxyalkylene copolymer
US4526780A (en) * 1981-03-09 1985-07-02 Colgate-Palmolive Company Anhydrous antiperspirant composition
US4499069A (en) * 1983-02-07 1985-02-12 The Gillette Company Antiperspirant emulsion
US4552753A (en) * 1983-12-01 1985-11-12 The Procter & Gamble Company Process for making roll-on antiperspirant compositions
US4782095A (en) * 1984-02-22 1988-11-01 Union Carbide Corporation Water-in-volatile silicone emulsifier concentrates
US4822603A (en) * 1986-06-18 1989-04-18 The Procter & Gamble Company Antiperspirant stick composition and process for preparing the same

Also Published As

Publication number Publication date
AU4725289A (en) 1990-07-19
JPH02229539A (en) 1990-09-12
EP0379677A3 (en) 1991-05-08
KR0154895B1 (en) 1998-12-01
US5008103A (en) 1991-04-16
ATE125171T1 (en) 1995-08-15
JPH0581292B2 (en) 1993-11-12
DE68923545T2 (en) 1996-02-15
AU631164B2 (en) 1992-11-19
EP0379677B1 (en) 1995-07-19
EP0379677A2 (en) 1990-08-01
ES2075030T3 (en) 1995-10-01
KR900009782A (en) 1990-07-05
DE68923545D1 (en) 1995-08-24

Similar Documents

Publication Publication Date Title
US5008103A (en) Silicone surfactants
EP0537003B1 (en) Silicone polyether alkyl copolymers
US6221927B1 (en) Polar solvent-in-oil emulsions and multiple emulsions
KR100421759B1 (en) Spontaneously formed transparent silicone micro-emulsion and method for forming the same
KR100270343B1 (en) Silicone contaning ole-in-water emulsions
DE60117602T2 (en) TRANSPARENT EMULSION HIGH OIL CONTENT WITH DIEN ELASTOMERS
US5066756A (en) Silicone surfactants
US5415860A (en) Cosmetic compositions comprising aqueous emulsions of organopolysiloxanes
KR100233322B1 (en) Stable water in oil emulsions
CN102026613A (en) Use of organo-modified siloxane block copolymers for producing cosmetic or pharmaceutical compositions
JPH02231416A (en) Perspiration inhibitor composition
CA1256381A (en) Water-in-volatile silicone emulsifier concentrates, water-in-volatile silicone emulsions that are useful in personal-care formulations and methods of making same
JPS6336620B2 (en)
EP1002825A2 (en) Non-aqueous silicone emulsions
MXPA03003487A (en) High oil clear emulsion with elastomer.
JPH02243612A (en) Cosmetic
JPH0748225A (en) Preparation of silicone-containing body care article and silicone composition
EP0377209A2 (en) Improved silicone surfactants
CA1166549A (en) Volatile silicone-water emulsions and methods of preparation and use
JPH0468015B2 (en)
JP2579516B2 (en) Hair cosmetics
US6410038B1 (en) Water-in-oil-in-polar solvent emulsions
JP5185111B2 (en) Oil absorption control method of silicone rubber powder
US5539136A (en) Silicone polyether surfactants synthesized using carbamate linkage
JP3135901B2 (en) Water-in-oil emulsion composition

Legal Events

Date Code Title Description
EEER Examination request
FZDE Discontinued