US20090056946A1 - Well remediation using downhole slurry - Google Patents
Well remediation using downhole slurry Download PDFInfo
- Publication number
- US20090056946A1 US20090056946A1 US12/111,948 US11194808A US2009056946A1 US 20090056946 A1 US20090056946 A1 US 20090056946A1 US 11194808 A US11194808 A US 11194808A US 2009056946 A1 US2009056946 A1 US 2009056946A1
- Authority
- US
- United States
- Prior art keywords
- component
- well
- cement
- density
- activator
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
A method of remediation of a well is provided utilizing a cement and cement activator plugging composition, in which one of the components is first placed in the well at the desired remediation depth. Next, the other component is placed in the well above the first placed component. Densities of the components have been selected such that the density of the second placed component is sufficiently higher then the density of the first placed component to facilitate gravity mixing of the two components as the second placed component moves through the first placed component and in the process activation occurs.
Description
- This application is a Continuation of U.S. patent application Ser. No. 11/162,444, filed Sep. 9, 2005, which issued Apr. 29, 2008 as U.S. Pat. No. 7,363,976, which claims priority/benefit of U.S. Provisional Patent Application Ser. Nos. 60/608,255, 60/608,256, and 60/608,257, all filed Sep. 9, 2004, with all the foregoing mentioned applications herein incorporated by reference.
- 1. Field of the Invention
- The present invention relates to wells, well operations, to methods, apparatus and products for operating wells. In another aspect, the present invention relates to wells, remediated wells, remediation of wells, to methods, apparatus and products for remediating wells, including oil, gas, water, geothermal, or analogous wells.
- 2. Brief Description of the Related Art
- The hard impermeable mass deposited in the annular space in a well by primary cementing processes is subjected to a number of stresses during the lifetime of the well. The pressure inside the casing can increase or decrease as the fluid filling it changes or as additional pressure is applied to the well, such as when the drilling fluid is replaced by a completion fluid or by a fluid used in a stimulation operation. A change of temperature also creates stress in the cement, at least during the transition period before the temperatures of the steel and the cement come into equilibrium. It can become necessary to repair the primary cementing mass.
- It is sometimes desirable in production of oil wells to place cement through perforations in the casing of the well both below and above the oil producing formation or zone. This cementing is carried out to prevent water and/or gas from migrating to the wellbore along with the oil. The intent is to leave the water and gas in the formations adjacent to the oil producing zone so that the water and gas will drive the oil to the wellbore, thereby increasing recovery of oil.
- Squeeze cementing is a process of forcing a cement composition through perforations, holes or splits in a casing/wellbore annular space of a well in order to repair a primary cement job that failed due to the cement bypassing the mud (channeling); to eliminate water intrusion from above, below or within the hydrocarbon-producing zone; to reduce the producing gas to oil ratio by isolating gas zones from adjacent oil intervals; to repair casing leaks due to a corroded or split pipe; to plug all, or part, of one or more zones in a multizone injection well so as to direct the injection into the desired intervals; and to plug and abandon a depleted or watered-out producing zone.
- Due to high pressures involved, squeeze cementing can be accompanied by problems such as propagating fractures. In addition, the use of conventional Portland cement has several potential problems of its own, particularly where high strength and good adhesion to the borehole wall are needed in order to effect good sealing. The presence of drilling mud pockets on channels under the primary cement may not only lead to failure of the primary cement job, but can adversely affect the strength of the squeeze cementing job. In addition, the presence of brine in the well can adversely affect both the primary and remedial cement jobs, increasing setting time and causing loss of strength of the cement.
- U.S. Pat. No. 5,178,519, issued Jan. 12, 1993, to Striech et al., discloses a method and apparatus for performing a block squeeze cementing job. The invention provides for perforating the wellbore above and below the desired well formation on a single wireline trip and setting a lower packer on a wireline above the lower perforations. A stinger is positioned in the lower packer, and secondary packer elements on an upper packer are set above the upper perforations. Cementing of the lower perforations is carried out through the lower packer. The secondary packer elements are unset, and the stinger is repositioned adjacent to the upper perforations. Primary packer elements on the upper packer are then set, and the cementing of the upper perforations is carried out through the upper packer and stinger. Setting of the secondary packer elements requires only vertical movement of the tubing string and no rotation. Both cementing steps are carried out on a single tubing trip. The upper packer is retrievable, and the lower packer is of a drillable type. Hydraulic slips may be provided on the upper packer to prevent movement thereof during either cementing operation.
- U.S. Pat. No. 6,065,539, issued May 23, 2000 to Noik et al., discloses a method of cementing a casing in a well drilled in the ground comprises injecting a liquid material comprising phenol-formol resin from the surface, wherein the resin is modified by means of a determined amount of furfuryl alcohol, and an amount of mineral filler unreactive towards the resin is added. The invention further relates to a thermosetting cementing material comprising phenol-formol resin. The resin is modified by means of an amount of furfuryl alcohol and comprises at least a proportion of an unreactive granular filler.
- U.S. Pat. No. 6,591,909, issued Jul. 15, 2003 to Dao et al., discloses a method and composition is provided using whey protein as a retarder in a cementing composition for use in cementing operations in a subterranean zone penetrated by a well bore.
- U.S. Pat. No. 6,767,867, issued Jul. 27, 2004 to Chatterji et al., discloses methods of treating subterranean zones penetrated by well bores in primary well cementing operations, well completion operations, production stimulation treatments and the like. The methods are basically comprised of introducing into the subterranean zone an aqueous well treating fluid comprised of water and a water soluble polymer complex fluid loss control additive.
- U.S. Pat. No. 6,899,177, issued May 31, 2005 to Chatterji et al., discloses methods of cementing subterranean zones penetrated by well bores using cement compositions having enhanced compressive strengths are provided. A method of the invention basically comprises the steps of preparing or providing a cement composition having enhanced compressive strength upon setting comprising a hydraulic cement, sufficient water to form a slurry and a hydroxyamine compressive strength enhancing additive. Thereafter, the cement composition is placed in a subterranean zone to be cemented and allowed to set into an impermeable solid mass therein.
- In spite of the advances in the prior art, conventional cement systems suffer from a 6 hour safety margin to dump the slurry; long set times; low shear bond values; long cement lengths, and long wait on cement (WOC) times causing high expense.
- Thus, there still exists a need in the art for improved methods, apparatus and products for remediating wells.
- According to one embodiment of the present invention, there is provided an active well (i.e, it's not abandoned) comprising a well bore; a first component residing in the wellbore; and, a second component having a density greater than the density of the first component, and positioned residing in the wellbore at a point above the first component that will allow for gravity flow of the second component down into the first component. The first component and the second component are selected from the group consisting of the cement component and the cement activator component, wherein the first component and the second component are different, and the density of the second component is higher than the density of the first component.
- According to even another embodiment of the present invention, there is provided a method of remediating an active well. The method includes providing a cement component and a cement activator component, each having a density greater than the density of any well fluid residing in the well. The method also includes selecting a first component and a second component from the group consisting of the cement component and the cement activator component, wherein the first component and the second component are different, and the density of the second component is higher than the density of the first component. The method even further includes placing the first component in the well. The method still further includes placing the second component in the well at a point above the first component that will allow for gravity flow of the second component down into contact with the first component.
- According to still another embodiment of the present invention, there is provided a method of remediating an active well. The method includes providing a cement component and a cement activator component, each having a density greater than the density of any well fluid residing in the well. The method also includes selecting a first component and a second component from the group consisting of the cement component and the cement activator component, wherein the first component and the second component are different, and the density of the second component is higher than the density of the first component. The method even further includes placing the first component in the well. The method still further includes placing the second component in the well at a point above the first component that will allow for gravity flow of the second component down into contact with the first component. The method yet further includes allowing the first and second components to gravity contact and form a cement plug.
- The method of the present invention for remediating an active well involves the use of a two part plugging composition, which is incorporated into known plugging methods. As used herein “active well” refers to any well that is not an abandoned well or one that is not undergoing abandonment. For example, a well during the process of drilling, an operating producing well, and the like.
- In particular, the preferred two part plugging composition of the present invention comprises a slurry system comprising a sealant component and an activator component.
- The slurry system utilized in the present invention may be any material suitable for forming a plug that will adequately plug the remediated well. Preferably, the sealant is a cement in the convention sense, that is, a silica based cement material of which Portland Cement is the best known example. Very well known in the prior art, Portland cement is manufactured by crushing, milling, and blending selected raw materials containing appropriate proportions of lime, iron, silica, and alumina, with certain Portland cements tailored specifically for plugging abandoned wells. Other hydraulic cements may be substituted for Portland cement. Activators for cements are well known, and any that are suitable for the particular well conditions and operation parameters may be utilized.
- In the present invention, the slurry system comprises not only cement and activator, but may optionally include additives to improve thermal stability, control set time, generate expansion, and control fluid loss. The additives may be present as independent components, or may be incorporated into the cement component or the activator component.
- As utilized in the present invention, the activator serves to activate/accelerate the set up or curing time for the cement and thus reduce the wait on cement (WOC) time. The activator causes the sealant to set under downhole temperature and pressure conditions at an accelerated rate. Of course, this activator will have to be carefully selected depending upon the material utilized as the first component.
- In the present invention, accelerated set times are generally less than 12 hours, preferably less than 10 hours, more preferably less than 8 hours, even more preferably less than 6 hours, still more preferably less than 4 hours, and yet more preferably less than 2 hours.
- The activator will cause the sealant to set under downhole conditions to cause the sealant to bond to the casing and or other formation surfaces in the well. The pipe may have coating of oil or water based drilling mud.
- The activator component may be selected to not only accelerate cement set, but may optionally be selected to also alter slurry density, clean downhole surfaces, and/or improve bond.
- Non-limiting examples cement activators suitable for use as the second component include various amines, non-limiting examples of which include triethanol amines and diethanol amines, various metal salts, non-limiting examples of which include sodium, calcium, magnesium, zine, and iron salts, various metal halides, including but not limited to metal chlorides and metal bromides, various formates, as well as combinations of the foregoing.
- For example, alkanolamines have been proposed for reducing the set time of cements, see U.S. Pat. Nos. 2,437,842; 3,553,077; 4,257,814, 4,741,782, and most recently 6,869,474, all herein incorporated by reference. As another example, bromide-based accelerators. In the practice of the present invention, where the first component is a cement, the second component preferably comprises an alkanolamine, more preferably comprises at least one selected from triethanolamine, diethanolamine, monoethanolamine and mixtures thereof, and even more preferably comprises triethanolamine.
- The method of the present invention for remediation of wells, includes any of the known remediation methods in which is utilized the two component plugging composition as the cement material. While a generalized remediation method is described below, it should be understood that any suitable remediation method as is known in the art, including any described above in the background or described in any cited reference (all of which are herein incorporated by reference), may be utilized with the plugging composition of the present invention.
- The cementing compositions of the invention are useful in a number of repair and remediation cementing operations including those operations to plug lost circulation and other undesirable fluid inflow and outflow zones in wells, to plug cracks and holes in pipe strings cemented therein and to accomplish other required remedial well operations. Generally, these repair and remediation cementing processes used in a well during its productive life are referred to as secondary cementing. In the practice of the present invention the compositions of the present invention may be utilized in any known secondary cementing method including any of the remediation cementing methods disclosed in any of the references cited herein, all of which are herein incorporated by reference.
- In general secondary cementing is carried out by placing components of a cementing composition from a source at the ground surface downhole to the point of repair and/or remediation. The components of the cementing composition are then allowed to set into a hard impermeable mass. Any method known in the art for placing and/or positioning components of a cementing composition downhole at the point of remediation may be used herein, all of which are herein incorporated by reference.
- Generally in the practice of the method of the present invention, one of the components is selected as the first placed component and placed in the well at the desired remediation location, followed by placement of the other component as the second placed component in the well at a position above the first component, to allow the second component to gravity flow into the first component.
- Preferable, in the practice of the present invention, the activator liquids are heavier than the well fluid and the cement component is heavier than the activator liquid.
- In general, suitable delivery systems utilize a dump bailer, coiled tubing and jointed tubing. They require a base to stack up against such as a packer, petal basket or sand plug. While any suitable delivery mechanism can be utilized, more specific non-limiting examples of suitable delivery mechanisms include: dump bailer run on electric line or slick line; pumping through tubing, drillpipe, work strings or any tubulars; allowing fall through fluids via gravity; and pumping into an annullas or pipe without displacing (i.e., “bull heading”).
- It is crucial that the first and second components have greater densities than the well fluid density. It is also crucial that the second placed component have a density greater than the first placed component so that the second placed component may displace the first component.
- In some instances the selected first and second components will not have suitable densities, specifically, the densities of the first and second components may not be greater than that of the well fluid, or they may not have the suitable density for the order in which they are desired to be introduced into the well, or the densities may not have a suitable enough differential to achieve suitable displacement.
- The present invention provides for the utilization of weighting agent additives to the first and second components to change the density of those components. Suitable additives to change the density include metal salts, preferably calcium chloride. Other examples of weighting agents include sand, barite, hemitite, calcium carbonate, FeO, MgO, and manganese ore. Sufficient amounts of the additive are utilized to achieve the desired density.
- In the remediation method of the present invention first and second components are provided which have densities greater than the well fluid, with the component to be placed second having a greater density than the component to be placed first. Should the density of the first or second component need adjustment, a weighting agent as discussed above, will be added as necessary. The component with the greater density is then introduced into the well fluid at a position on top of sand/petal basket, the other component is then placed above the first placed component so that it may spontaneously gravity flow into contact the first placed fluid. The density difference will allow displacement of the first placed fluid by the second placed fluid and allow for in-situ mixing.
- It should be appreciated that the rate of displacement and thus in-situ mixing will increase with increasing density differential between the first and second components, and decrease with decreasing density differential between the first and second components.
- It should also be appreciated that at some point, the density differential between the first and second components is so low as to result in too slow of displacement.
- On the other hand, it should further be appreciated that at some point, the density differential between the first and second components is so great as to result in too rapid of displacement so as to avoid much mixing.
- Thus, the density differential should be selected so as to provide fast enough displacement for the plugging operation, and to facilitate sufficient in-situ mixing, and this differential can be determined on a case by case basis, for example by observation in clear container and trial and error.
- Typical densities for the well fluid will be in the range of about 8.33 ppg up to about 20.0 ppg, with typical densities for the activator in the range of about 8.33 ppg up to about 21.0 ppg, and with typical densities for the sealant system in the range of about 8.54 up to about 22.0 ppg.
- It should be understood that other well fluid additives as are well known in the art may be incorporated into the first and/or second component, or added before, along with, or after the introduction of the first and/or second component, non-limiting examples of which include surfactants, surface bond enhancers (non-limiting examples include styrene butadiene latex, polyvinal alcohols, resins, other adhesives), emulsifiers, ph control agents, fluid loss additives, gas prevention additive, dispersants, expanding agents, and wetting agents.
- It should also be understood that the activator viscosity and missibility much be such that the activator will not substantially mix with the well fluid as it passes thru the well fluid. Preferably, the activator viscosity and missibility much be such that the activator will mixes less than 20% with the well fluid as it falls through it, more preferably less than 10%, and even more preferably less than 2%.
- It should be further understood that activator and sealant viscosities and missibility are such that the activator mixes less than 40% with the sealant as they contact each other, preferably less then 20%, more preferably less than 10%, and even more preferably less than 5%.
- Although the present invention has been illustrated by reference to cement, especially Portland cement, and to an activator therefore, it should be understood that any plugging composition having two or more components can be utilized in the present invention.
- All materials cited herein, including but not limited to any cited patents, publications, articles, books, journals, brochures, are herein incorporated by reference.
- While the illustrative embodiments of the invention have been described with particularity, it will be understood that various other modifications will be apparent to and can be readily made by those skilled in the art without departing from the spirit and scope of the invention. Accordingly, it is not intended that the scope of the claims appended hereto be limited to the examples and descriptions set forth herein but rather that the claims be construed as encompassing all the features of patentable novelty which reside in the present invention, including all features which would be treated as equivalents thereof by those skilled in the art to which this invention pertains.
Claims (14)
1. A method of remediating a well having a well fluid residing in the well, the method comprising:
(A) providing a cement component and an cement activator component, each having a density greater than the density of the well fluid;
(B) selecting a first component and a second component from the group consisting of the cement component and the cement activator component, wherein the first component and the second component are different, and the density of the second component is higher than the density of the first component;
(C) placing the first component in the well to be remediated;
(D) placing the second component in the well at a point above the first component that will allow for gravity flow of the second component down into contact with the first component.
2. The method of claim 1 , wherein steps (C) and (D) are carried out utilizing one or more of a dump bailer; pumping through tubing, drillpipe, work strings or tubulars; gravity flow; and bull heading.
3. The method of claim 1 , wherein the activator component comprises at least one selected from the group consisting of amines, metal salts, metal halides, and formats.
4. The method of claim 1 , wherein the second component is the cement component, and the first component is the activator component.
5. The method of claim 1 , wherein the well fluid density is in the range of about 8.33 ppg up to about 20.0 ppg, the activator density is in the range of about 8.33 ppg up to about 21.0 ppg, and the cement density is in the range of about 8.54 up to about 22.0 ppg.
6. The method of claim 1 , wherein the activator mixes with less than 2 percent with the well fluid, and the activator mixes with less than 20% with the cement.
7. A method of remediating a well having a well fluid residing therein, the method comprising:
(A) providing a cement component and an cement activator component, each having a density greater than the density of the well fluid;
(B) selecting a first component and a second component from the group consisting of the cement component and the cement activator component, wherein the first component and the second component are different, and the density of the second component is higher than the density of the first component;
(C) placing the first component in the well to be remediated;
(D) placing the second component in the well at a point above the first component that will allow for gravity flow of the second component down into the first component; and
(E) allowing the first and second components to gravity contact and form a cement plug.
8. The method of claim 7 , wherein steps (C) and (D) are carried out utilizing one or more of a dump bailer; pumping through tubing, drillpipe, work strings or tubulars; gravity flow; and bull heading.
9. The method of claim 7 , wherein the activator component comprises at least one selected from the group consisting of amines, metal salts, metal halides, and formats.
10. The method of claim 7 , wherein the second component is the cement component, and the first component is the activator component.
11. The method of claim 7 , wherein the well fluid density is in the range of about 8.33 ppg up to about 20.0 ppg, the activator density is in the range of about 8.33 ppg up to about 21.0 ppg, and the cement density is in the range of about 8.54 up to about 22.0 ppg.
12. The method of claim 7 , wherein the activator mixes with less than 2 percent with the well fluid, and the activator mixes with less than 20% with the cement.
13. A remediated well comprising:
a well bore of an active well;
a first component residing in the well bore; and,
a second component having a density greater than the density of the first component, and residing in the wellbore at a point above the first component that will allow for gravity flow of the second component down into the first component, wherein one of the first component and the second component is a cement component, and the other of the first component and second component is a cement activator component.
14. A remediated well comprising:
a well bore of an active well;
a first component residing in the well bore; and,
a second component having a density greater than the density of the first component, and in the state of gravity flowing thru the first component, wherein one of the first component and the second component is a cement component, and the other of the first component and second component is a cement activator component.