WO2005071217A1 - Methods, compositions and biodegradable fluid loss control additives for cementing subterranean zones - Google Patents

Methods, compositions and biodegradable fluid loss control additives for cementing subterranean zones Download PDF

Info

Publication number
WO2005071217A1
WO2005071217A1 PCT/GB2004/004522 GB2004004522W WO2005071217A1 WO 2005071217 A1 WO2005071217 A1 WO 2005071217A1 GB 2004004522 W GB2004004522 W GB 2004004522W WO 2005071217 A1 WO2005071217 A1 WO 2005071217A1
Authority
WO
WIPO (PCT)
Prior art keywords
weight
condensation product
water
formaldehyde
sodium sulfite
Prior art date
Application number
PCT/GB2004/004522
Other languages
French (fr)
Inventor
Jiten Chatterji
Roger S. Cromwell
Bobby J. King
Darrell Chad Brenneis
Original Assignee
Halliburton Energy Services, Inc.
Wain, Christopher, Paul
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Halliburton Energy Services, Inc., Wain, Christopher, Paul filed Critical Halliburton Energy Services, Inc.
Publication of WO2005071217A1 publication Critical patent/WO2005071217A1/en

Abstract

Methods, compositions and fluid loss control additives for cementing in subterranean zones are disclosed. A cement composition comprises a hydraulic cement, sufficient water to form a slurry and a water soluble biodegradable fluid loss control additive comprising a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide.

Description

METHODS, COMPOSITIONS AND BIODEGRADABLE FLUID LOSS CONTROL ADDITIVES FOR CEMENTING SUBTERRANEAN ZONES
BACKGROUND OF THE INVENTION
1. FIELD OF THE INVENTION The present invention relates to improved methods, compositions and fluid loss control additives for cementing subterranean zones penetrated by well bores.
2. DESCRIPTION OF THE PRIOR ART Subterranean zones penetrated by well bores are commonly sealed by hydraulic cement compositions. For example, hydraulic cement compositions are used in primary cementing operations whereby strings of pipe such as casing and liners are cemented in well bores. In performing primary cementing, a hydraulic cement composition is pumped into the annular space between walls of a well bore and the exterior surfaces of a pipe string disposed therein. The cement composition is permitted to set in the annular space thereby forming an annual sheath of hardened substantially impermeable cement therein which supports and positions the pipe string in the well bore and seals the exterior surfaces of the pipe string to the walls of the well bore. Hydraulic cement compositions are also utilized in a variety of cementing operations such as sealing highly permeable zones or fractures in subterranean zones, plugging cracks or holes in pipe strings and the like. Fluid loss control additives have been included in hydraulic cement compositions to prevent significant loss of fluid, i.e. water, into the subterranean zone or formation being cemented. In primary cementing, the loss of fluid from the cement composition can result in premature gelation of the cement slurry or bridging of the annular space between the formation and the casing. While a variety of fluid loss control additives have been utilized in hydraulic cement slurries used in cementing subterranean zones penetrated by well bores, they are not environmentally acceptable, especially in off shore operations in that they do not undergo complete biodegration in the environment and cause damage to aquatic and other life therein. Thus, there are continuing needs for improved biodegradable cement composition fluid loss control additives and improved cement compositions containing such additives. SUMMARY OF THE INVENTION The present invention provides improved methods, compositions and biodegradable fluid loss control additives for cementing subterranean zones that meet the needs described above and overcome the deficiencies of the prior art. The methods of the invention for cementing subterranean zones penetrated by a well bore basically comprise the following steps. A cement composition comprising a hydraulic cement, sufficient water to form a slurry and a water soluble biodegradable fluid loss control additive is prepared or provided. The biodegradable fluid loss control additive comprises a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide with a molar substitution of about 1.5 moles being preferred. Examples of the condensation products that can be used include, but are not limited to: water, gelatin, formaldehyde, sodium sulfite and acetone; water, casein, formaldehyde, sodium sulfite and acetone; casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfϊte; water, soy protein, formaldehyde, sodium sulfite and acetone; water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol; dimethylsulfoxide, gelatin, glyoxal, urea and sodium sulfite; and water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide. The cement composition is placed in the subterranean zone to be cemented, and then the cement composition is allowed to set into a solid mass therein. The well cement compositions of this invention basically comprise a hydraulic cement, sufficient water to form a slurry and a water soluble biodegradable cement fluid loss control additive comprising a mixture of a condensation product as described above and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide. The water soluble biodegradable fluid loss control additives of this invention comprise a mixture of a condensation product as described above and hydroxyethylcellulose having a molar substitution in the range of from about 1 to about 2.5 moles of ethylene oxide. The objects, features and advantages of the present invention will be readily apparent to those skilled in the art upon a reading of the description of preferred embodiments which follows. DESCRIPTION OF PREFERRED EMBODIMENTS The methods of cementing a subterranean zone penetrated by a well bore in accordance with the present invention comprise the following steps. A cement composition is prepared or provided comprising a hydraulic cement, sufficient water to form a slurry and a water soluble biodegradable fluid loss control additive. The cement composition is placed in the subterranean zone to be cemented and the cement composition is then allowed to set into a solid mass therein. The cement compositions of this invention basically comprise a hydraulic cement, sufficient water to form a slurry, and a water soluble biodegradable fluid loss control additive. The hydraulic cements that can be utilized in the compositions of this invention include, but are not limited to, Portland cements, slag cements, pozzolana cements, gypsum cements, aluminous cements and silica cements. Of these, Portland cements and their equivalents are generally preferred for use in accordance with this invention. The water in the cement compositions can be fresh water or salt water. The term "salt water" is used herein to mean unsaturated salt solutions and saturated salt solutions including brines and seawater. The water is present in the cement compositions in amounts sufficient to form a pumpable slurry. Generally, the water is present in an amount in the range of from about 35% to about 65% by weight of hydraulic cement in the compositions. The water soluble biodegradable fluid loss control additives comprise a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 to about 2.5 moles of ethylene oxide, preferably about 1.5 moles. Examples of the condensation products that can be used and their preparation include, but are not limited to, the following: (No. 1) The condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone. A preferred such condensation product comprises 43.17% by weight water, 17.27% by weight gelatin, 25.18% by weight formaldehyde, 7.19% by weight sodium sulfite and 7.19% by weight acetone. The condensation product is prepared by dissolving 240 grams of gelatin in 600 grams of water containing 100 grams of sodium sulfite and 100 grams of acetone. Following the addition of 350 grams of a 37% by weight aqueous formaldehyde solution, the mixture is heated to 140°F. The pH of the solution is adjusted to 7 with formic acid and heated for two hours at 176°F. The reaction solution is distilled in a vacuum to remove methanol produced by the competing Canizarro reaction. (No. 2) The condensation product of water, casein, formaldehyde, sodium sulfite and acetone. A preferred such condensation product comprises 61.05% by weight water, 5.81% by weight casein, 23.26% by weight formaldehyde, 5.08% by weight sodium sulfite and 4.80% by weight acetone. The condensation product is prepared by dissolving 20 grams of casein in 210 grams of water. 17.5 grams of sodium sulfite and 16.5 grams of acetone are added to the casein solution. The solution is heated to 140°F followed by slow addition of 80 grams of 30% aqueous formaldehyde solution. The solution is stirred for two hours at 158°F and the pH of the reaction solution is adjusted to 7 with formic acid. The solution is then concentrated to half the original volume by vacuum distillation to remove methanol. (No. 3) The condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite. A preferred such condensation product comprises 26.90% by weight casein, 7.91% by weight sodium sulfite, 7.91% by weight acetone, 19.77% by weight water, 36.94% by weight formaldehyde and 0.57% by weight sodium pyrosulfite. The condensation product is prepared by dissolving 100 grams of sodium sulfite and 100 grams of acetone in 250 grams of water. The solution is heated to 140°F. Then 467 grams of 30% aqueous formaldehyde solution are added. The reaction solution is stirred for 40 minutes at 158°F. At the end of 40 minutes, 7.26 grams of sodium pyrosulfite are added and the solution is stirred for an additional 30 minutes. The pH of the solution is adjusted to 7.0 with formic acid. The solution is distilled under vacuum to remove methanol. The residual solution is diluted to 6 liters with distilled water and 340 grams of casein. The resulting polymer solution is dried whereby grafting of the backbone takes place. (No. 4) The condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone. A preferred such condensation product comprises 47.69% by weight water, 7.95% by weight soy protein, 8.27% by weight sodium sulfite, 7.79% by weight acetone, and 28.30% by weight formaldehyde. The condensation product is prepared by adding 100 grams of soy protein to 600 grams of water. The pH of the solution is adjusted to about 13 with sodium hydroxide. To this solution are added 104 grams of sodium sulfite and 98 grams of acetone. The mixture is then heated to 176°F. To the heated solution 356 grams of 30% aqueous formaldehyde solution are added drop wise with vigorous agitation. The pH of the solution is adjusted to 7 with formic acid. Methanol produced by a competing Canizarro reaction is completely distilled off under vacuum to produce the condensation product. (No. 5) The condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol. A preferred such condensation product comprises 43.94% by weight water, 6.99% by weight polyaspartic acid, 17.96% by weight acetaldehyde, 34.80% by weight sodium sulfite and 36.00% by weight pyrocatechol. The condensation product is prepared by dissolving 15.9 grams of polyaspartic acid in 100 grams of water. The solution is cooled to 35.6°F. To the chilled solution is added 34.8 grams of sodium sulfite and 36 grams of pyrocatechol. Then, 40.9 grams of acetaldehyde is added drop wise taking precaution not to raise the temperature of the solution above 53.6°F. Upon completion of the addition, the temperature is raised to 167°F and agitated for two hours at that temperature. The solution is cooled to 68°F and the pH is adjusted to 7 by formic acid. The solution is concentrated to half its volume under vacuum. (No. 6) The condensation product of dimethylsulfoxide, gelatin, glyoxal, urea, and sodium sulfite. A preferred such condensation product comprises 57.75% by weight dimethylsulfoxide, 20.88% by weight gelatin, 3.62% by weight glyoxal, 8.61% by weight urea, and 17.40% by weight sodium sulfite. The condensation product is prepared by adding 39.77 grams of gelatin to 100 milliliters of dimethyl sulfoxide. To the solution is added 17.4 grams of sodium sulfite and 16.4 grams of urea with stirring. The mixture is heated to 140°F, followed by the addition of 6.9 grams of 40% aqueous glyoxal solution. The reaction mixture is then heated to 167°F and held at that temperature for two hours. The dimethyl sulfoxide is then removed under reduced pressure. (No. 7) The condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide. A preferred such condensation product comprises 39.55% by weight water, 9.88% by weight polyaspartic acid, 21.19% by weight formaldehyde, 7.06% by weight sodium pyrosulfite, 8.90% by weight melamine, and 13.42% by weight sodium hydroxide. The condensation product is prepared by heating 150 grams of 30% aqueous formaldehyde solution to 86°F. Then, 63 grams of melamine and 50 grams of sodium pyrosulfite are added, followed by 95 grams of a 15% solution of sodium hydroxide. To this solution is added 280 grams of water. The pH of the solution is adjusted to 3 with sulfuric acid. 70 grams of a 40% aqueous solution of polyaspartic acid is then added to the solution. The solution is raised to a temperature of 160°F and held at that temperature for two hours. The reaction solution is concentrated to 1/3 of its original volume with reduced pressure and a temperature of 176°F. The solution is cooled and the pH is adjusted to 7 with sodium hydroxide. Of the above condensation products, the condensation product (No. 1) comprising water, gelatin, formaldehyde, sodium sulfite and acetone is preferred. The condensation product comprises from about 70% to about 90% by weight of the water soluble biodegradable fluid loss control additive and the hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide comprises from about 10% to about 30% by weight thereof. More preferably, the condensation product comprises about 80% by weight of the water soluble biodegradable fluid loss control additive and the hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide comprises about 20% by weight thereof. Most preferably, the water soluble biodegradable fluid loss control additive comprises the condensation product of gelatin, acetone, formaldehyde and sodium sulfite in an amount of about 80% by weight of the additive and hydroxyethylcellulose having a molar substitution of about 1.5 moles of ethylene oxide in an amount of about 20% by weight of the additive. The water soluble biodegradable fluid loss control additive is present in the cement composition in an amount in the range of from about 0.5% to about 2% by weight of cement therein, more preferably in an amount of about 1% by weight of cement therein. A preferred method of this invention for cementing a subterranean zone penetrated by a well bore comprises the steps of: (a) preparing or providing a cement composition that comprises a hydraulic cement, sufficient water to form a slurry and a water soluble biodegradable fluid loss control additive comprising a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide; (b) placing the cement composition in the subterranean zone to be cemented; and (c) allowing the cement composition to set into a solid mass therein. A preferred well cement composition of this invention comprises: a hydraulic cement; sufficient water to form a slurry; and a water soluble biodegradable fluid loss control additive comprising a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide. A preferred water soluble biodegradable fluid loss control additive of this invention comprises a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide. In order to further illustrate the methods and compositions of this invention, the following examples are given. EXAMPLE 1 Two water soluble biodegradable fluid loss control additives of this invention were prepared. The first fluid loss control additive comprised a mixture of the condensation product of gelatin, acetone, formaldehyde and sodium sulfite present in an amount of 90% by weight and hydroxyethylcellulose having a molar substitution of 1.5 moles of ethylene oxide present in an amount of 10% by weight. The second fluid loss control additive comprised a mixture of the condensation product of gelatin, acetone, formaldehyde and sodium sulfite present in an amount of 80% by weight and hydroxyethylcellulose having a molar substitution of 1.5 moles of ethylene oxide present in an amount of 20% by weight. The first and second biodegradable fluid loss control additives of this invention along with a non- biodegradable prior art fluid loss control additive were tested for fluid loss control properties in accordance with the test procedure set forth in the API Specification for Materials and Testing for Well Cements, API Specification 10B, 22nd Edition, dated December, 1997 of the American Petroleum Institute. The non-biodegradable prior art fluid loss control additive was compared to the two fluid loss control additives of this invention. The results of these tests are given in Table I below. TABLE I Comparison of Fluid Loss Control Properties
Figure imgf000009_0001
Condensation product of formaldehyde, acetone and sodium bisulfite (80% by weight) and hydroxyethylcellulose having a molar substitution of 1.5 moles of ethylene oxide (20% by weight). See U.S. Patent No. 4,557,763 issued to George, et al. on December 10, 1985. ' Condensation product of gelatin, acetone, formaldehyde and sodium sulfite (90%) and hydroxyethylcellulose having a molar substitution of 1.5 moles of ethylene oxide (10%). Condensation product of gelatin, acetone, formaldehyde and sodium sulfite (80%) and hydroxyethylcellulose having a molar substitution of 1.5 moles of ethylene oxide (20%). From Table I, it can be seen that the non-biodegradable prior art fluid loss control additive and the second biodegradable fluid loss control additive of this invention have comparable fluid loss control properties. EXAMPLE 2 The non-biodegradable prior art fluid loss control additive and the second biodegradable fluid loss control additive were combined with cement compositions in an amount 1% by weight of the cement. One of the cement compositions contained fresh water and the other contained fresh water with 18% by weight of salt added thereto. The results of these tests are given in Table π below. TABLE II Comparison of Rheological Properties
Figure imgf000010_0001
From Table II, it can be seen that the rheological properties of the two fluid loss control additives are comparable irrespective of temperature. In the cement composition containing salt, the rheological properties of the two mixtures were similar. EXAMPLE 3 The non-biodegradable prior art fluid loss control additive and the second biodegradable fluid loss control additive of this invention were added to cement compositions and the compositions were tested for thickening time. The results of these tests are given in Table HI below. TABLE III Comparison of Thickening Times
Figure imgf000011_0001
From Table III, it can be seen that the thickening times of the fluid loss control additives at 100°F and 140°F were comparable. EXAMPLE 4 The non-biodegradable prior art fluid loss control additive and the second biodegradable fluid loss control additive of this invention were added to cement compositions and the cement compositions were cured at 140°F for 24 hours and 72 hours and were then tested for compressive strength. TABLE IN Comparison of 140°F Compressive Strengths
Figure imgf000011_0002
From Table IN, it can be seen that the cement composition containing the non- biodegradable prior art fluid loss control additive and the biodegradable fluid loss control additive have similar compressive strengths. Thus, the present invention is well adapted to carry out the objects and attain the ends and advantages mentioned as well as those which are inherent therein. While numerous changes may be made by those skilled in the art, such changes are encompassed within the spirit of this invention as defined by the appended claims.

Claims

What is claimed is:
1. A method of cementing in a subterranean zone comprising: preparing or providing a cement composition that comprises a hydraulic cement, sufficient water to form a slurry and a water soluble biodegradable fluid loss control additive comprising a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide; placing the cement composition in the subterranean zone to be cemented; and allowing the cement composition to set therein.
2. The method of claim 1 wherein the hydraulic cement in the cement composition is selected from the group consisting of Portland cements, slag cements, pozzolana cements, gypsum cements, aluminous cements and silica cements.
3. The method of claim 1 wherein the hydraulic cement in the cement composition is Portland cement.
4. The method of claim 1 wherein the water in the cement composition is selected from the group consisting of fresh water and salt water.
5. The method of claim 1 wherein the water is present in the cement composition in an amount in the range of from about 35% to about 65% by weight of cement therein.
6. The method of claim 1 wherein the condensation product is selected from the group consisting of the condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone; the condensation product of water, casein, formaldehyde, sodium sulfite and acetone; the condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite; the condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone; the condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol; the condensation product of dimethylsulfoxide, gelatin, glyoxal, urea and sodium sulfite; and the condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide.
7. The method of claim 1 wherein the condensation product is the condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone.
8. The method of claim 7 wherein the condensation product comprises 43.17% by weight water, 17.27% by weight gelatin, 25.18% by weight formaldehyde, 7.19% by weight sodium sulfite and 7.19% by weight acetone.
9. The method of claim 1 wherein the condensation product is the condensation product of water, casein, formaldehyde, sodium sulfite and acetone.
10. The method of claim 9 wherein the condensation product comprises 61.05% by weight water, 5.81% by weight casein, 23.26% by weight formaldehyde, 5.08% by weight sodium sulfite and 4.80% by weight acetone.
11. The method of claim 1 wherein the condensation product is the condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite.
12. The method of claim 11 wherein the condensation product comprises 26.90% by weight casein, 7.91% by weight sodium sulfite, 7.91% by weight acetone, 19.77% by weight water, 36.94% by weight formaldehyde and 0.57% by weight sodium pyrosulfite.
13. The method of claim 1 wherein the condensation product is the condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone.
14. The method of claim 13 wherein the condensation product comprises 47.69% by weight water, 7.95% by weight soy protein, 8.27% by weight sodium sulfite, 7.79% by weight acetone, and 28.30% by weight formaldehyde.
15. The method of claim 1 wherein the condensation product is the condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol.
16. The method of claim 15 wherein the condensation product comprises 43.94% by weight water, 6.99% by weight polyaspartic acid, 17.96% by weight acetaldehyde, 34.80% by weight sodium sulfite and 36.00% by weight pyrocatechol.
17. The method of claim 1 wherein the condensation product is the condensation product of dimethylsulfoxide, gelatin, glyoxal, urea, and sodium sulfite.
18. The method of claim 17 wherein the condensation product comprises 57.75% by weight dimethylsulfoxide, 20.88% by weight gelatin, 3.62% by weight glyoxal, 8.61% by weight urea, and 17.40% by weight sodium sulfite.
19. The method of claim 1 wherein the condensation product is the condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide.
20. The method of claim 19 wherein the condensation product comprises 39.55% by weight water, 9.88% by weight polyaspartic acid, 21.19% by weight formaldehyde, 7.06% by weight sodium pyrosulfite, 8.90% by weight melamine, and 13.42% by weight sodium hydroxide.
21. The method of claim 1 wherein the water soluble biodegradable fluid loss control additive comprises a condensation product in the range of from about 70% to about 90% by weight thereof and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide in the range of from about 10% to about 30% by weight thereof.
22. The method of claim 1 wherein the water soluble biodegradable fluid loss control additive comprises the condensation product of gelatin, formaldehyde, sodium sulfite and acetone in an amount of about 80% by weight thereof and hydroxyethylcellulose having a molar substitution of from about 1.5 moles of ethylene oxide in an amount of about 20% by weight thereof.
23. The method of claim 1 wherein the water soluble biodegradable fluid loss control additive is present in the cement composition in an amount in the range of from about 0.5% to about 2% by weight of cement therein.
24. A cement composition comprising: a hydraulic cement; sufficient water to form a slurry; and a water soluble biodegradable fluid loss control additive comprising a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide.
25. The cement composition of claim 24 wherein the hydraulic cement in the cement composition is selected from the group consisting of Portland cements, slag cements, pozzolana cements, gypsum cements, aluminous cements and silica cements.
26. The cement composition of claim 24 wherein the hydraulic cement in the cement composition is Portland cement.
27. The cement composition of claim 24 wherein the water in the cement composition is selected from the group consisting of fresh water and salt water.
28. The cement composition of claim 24 wherein the water is present in the cement composition in an amount in the range of from about 35% to about 65% by weight of cement therein.
29. The cement composition of claim 24 wherein the condensation product is selected from the group consisting of the condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone; the condensation product of water, casein, formaldehyde, sodium sulfite and acetone; the condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite; the condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone; the condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol; the condensation product of dimethylsulfide, gelatin, glyoxal, urea and sodium sulfite; and the condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hdyroxide.
30. The cement composition of claim 24 wherein the condensation product is the condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone.
31. The cement composition of claim 24 wherein the condensation product comprises 43.17% by weight water, 17.27% by weight gelatin, 25.18% by weight formaldehyde, 7.19% by weight sodium sulfite and 7.19% by weight acetone.
32. The cement composition of claim 24 wherein the condensation product is the condensation product of water, casein, formaldehyde, sodium sulfite and acetone.
33. The cement composition of claim 32 wherein the condensation product comprises 61.05% by weight water, 5.81% by weight casein, 23.26% by weight formaldehyde, 5.08% by weight sodium sulfite and 4.80% by weight acetone.
34. The cement composition of claim 24 wherein the condensation product is the condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite.
35. The cement composition of claim 34 wherein the condensation product comprises 26.90% by weight casein, 7.91% by weight sodium sulfite, 7.91% by weight acetone, 19.77% by weight water, 36.94% by weight formaldehyde and 0.57% by weight sodium pyrosulfite.
36. The cement composition of claim 24 wherein the condensation product is the condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone.
37. The cement composition of claim 36 wherein the condensation product comprises 47.69% by weight water, 7.95% by weight soy protein, 8.27% by weight sodium sulfite, 7.79% by weight acetone, and 28.30% by weight formaldehyde.
38. The cement composition of claim 24 wherein the condensation product is the condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol.
39. The cement composition of claim 38 wherein the condensation product comprises 43.94% by weight water, 6.99% by weight polyaspartic acid, 17.96% by weight acetaldehyde, 34.80% by weight sodium sulfite and 36.00% by weight pyrocatechol.
40. The cement composition of claim 24 wherein the condensation product is the condensation product of dimethylsulfoxide, gelatin, glyoxal, urea, and sodium sulfite.
41. The cement composition of claim 40 wherein the condensation product comprises 57.75% by weight dimethylsulfoxide, 20.88% by weight gelatin, 3.62% by weight glyoxal, 8.61% by weight urea, and 17.40% by weight sodium sulfite.
42. The cement composition of claim 24 wherein the condensation product is the condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide.
43. The cement composition of claim 42 wherein the condensation product comprises 39.55% by weight water, 9.88% by weight polyaspartic acid, 21.19% by weight formaldehyde, 7.06% by weight sodium pyrosulfite, 8.90% by weight melamine, and 13.42% by weight sodium hydroxide.
44. The cement composition of claim 24 wherein the water soluble biodegradable fluid loss control additive comprises a condensation product in the range of from about 70% to about 90% by weight thereof and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide in the range of from about 10%) to about 30% by weight thereof.
45. The cement composition of claim 24 wherein the water soluble biodegradable fluid loss control additive comprises the condensation product of gelatin, formaldehyde, sodium sulfite and acetone in an amount of about 80% by weight thereof and hydroxyethylcellulose having a molar substitution of from about 1.5 moles of ethylene oxide in an amount of about 20% by weight thereof.
46. The cement composition of claim 24 wherein the water soluble biodegradable fluid loss control additive is present in the cement composition in an amount in the range of from about 0.5% to about 2% by weight of cement therein.
47. A water soluble biodegradable fluid loss control additive comprising a mixture of a condensation product and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide.
48. The additive of claim 47 wherein the condensation product is selected from the group consisting of the condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone; the condensation product of water, casein, formaldehyde, sodium sulfite and acetone; the condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite; the condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone; the condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol; the condensation product of dimethylsulfide, gelatin, glyoxal, urea and sodium sulfite; and the condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide.
49. The additive of claim 47 wherein the condensation product is the condensation product of water, gelatin, formaldehyde, sodium sulfite and acetone.
50. The additive of claim 47 wherein the condensation product comprises 43.17% by weight water, 17.27% by weight gelatin, 25.18% by weight formaldehyde, 7.19% by weight sodium sulfite and 7.19% by weight acetone.
51. The additive of claim 47 wherein the condensation product is the condensation product of water, casein, formaldehyde, sodium sulfite and acetone.
52. The additive of claim 51 wherein the condensation product comprises 61.05% by weight water, 5.81% by weight casein, 23.26% by weight formaldehyde, 5.08% by weight sodium sulfite and 4.80% by weight acetone.
53. The additive of claim 47 wherein the condensation product is the condensation product of casein, sodium sulfite, acetone, water, formaldehyde and sodium pyrosulfite.
54. The additive of claim 53 wherein the condensation product comprises 26.90% by weight casein, 7.91% by weight sodium sulfite, 7.91% by weight acetone, 19.77% by weight water, 36.94% by weight formaldehyde and 0.57% by weight sodium pyrosulfite.
55. The additive of claim 47 wherein the condensation product is the condensation product of water, soy protein, formaldehyde, sodium sulfite and acetone.
56. The additive of claim 55 wherein the condensation product comprises 47.69% by weight water, 7.95% by weight soy protein, 8.27% by weight sodium sulfite, 7.79% by weight acetone, and 28.30% by weight formaldehyde.
57. The additive of claim 47 wherein the condensation product is the condensation product of water, polyaspartic acid, acetaldehyde, sodium sulfite and pyrocatechol.
58. The additive of claim 57 wherein the condensation product comprises 43.94% by weight water, 6.99% by weight polyaspartic acid, 17.96% by weight acetaldehyde, 34.80% by weight sodium sulfite and 36.00% by weight pyrocatechol.
59. The additive of claim 47 wherein the condensation product is the condensation product of dimethylsulfoxide, gelatin, glyoxal, urea, and sodium sulfite.
60. The additive of claim 59 wherein the condensation product comprises 57.75% by weight dimethylsulfoxide, 20.88% by weight gelatin, 3.62% by weight glyoxal, 8.61% by weight urea, and 17.40% by weight sodium sulfite.
61. The additive of claim 47 wherein the condensation product is the condensation product of water, polyaspartic acid, formaldehyde, sodium pyrosulfite, melamine and sodium hydroxide.
62. The additive of claim 61 wherein the condensation product comprises 39.55% by weight water, 9.88% by weight polyaspartic acid, 21.19% by weight formaldehyde, 7.06% by weight sodium pyrosulfite, 8.90% by weight melamine, and 13.42% by weight sodium hydroxide.
63. The additive of claim 23 wherein the water soluble biodegradable fluid loss control additive comprises a condensation product in the range of from about 70% to about 90% by weight thereof and hydroxyethylcellulose having a molar substitution in the range of from about 1 mole to about 2.5 moles of ethylene oxide in the range of from about 10% to about 30% by weight thereof.
64. The additive of claim 23 wherein the water soluble biodegradable fluid loss control additive comprises the condensation product of gelatin, formaldehyde, sodium sulfite and acetone in an amount of about 80% by weight thereof and hydroxyethylcellulose having a molar substitution of from about 1.5 moles of ethylene oxide in an amount of about 20% by weight thereof.
65. The additive of claim 23 wherein the water soluble biodegradable fluid loss control additive is present in the cement composition in an amount in the range of from about 0.5% to about 2% by weight of cement therein.
PCT/GB2004/004522 2004-01-21 2004-10-26 Methods, compositions and biodegradable fluid loss control additives for cementing subterranean zones WO2005071217A1 (en)